In the Basic Oxygen Steelmaking context, refining high-silicon hot metal is an awkward operation due to the significant tendency to slopping that it points out. At Steelworks n° 2 of ILVA steel plant situated in Taranto, this problem is solved by a double-slag operation. In the present work we have defined a new operating practice that, without the double-slag operation, achieves a reduction in the tap to tap time and a greater process gases recovery, without affecting the neither the slopping control nor the quality of steel obtained at the end of the blow. The feasibility of such a new practice was verified through a critical analysis of the results obtained from thirty experimental tests carried out at ILVA Steelworks n° 2 converters.
Nel contesto dell’acciaieria a ossigeno, l’affinazione in convertitore di ghisa ad elevato contenuto di silicio risulta un’operazione piuttosto delicata a causa della significativa tendenza allo slopping che essa fa rilevare. Presso l’Acciaieria 2 dello stabilimento siderurgico ILVA di Taranto, tale problematica è risolta effettuando una doppia scorifica. Nel presente lavoro si è definita una nuova pratica operativa che, senza ricorrere alla doppia scorifica, consente di ottenere una riduzione del tempo di tap to tap e un maggiore recupero dei gas di processo, senza inficiare il controllo dello slopping né la qualità dell’acciaio ottenuto. L’applicabilità di tale pratica è stata verificata mediante un’analisi critica dei risultati di trenta prove sperimentali svolte presso i convertitori dell’Acciaieria 2 ILVA.
Studio di una nuova pratica operativa per l'affinazione al convertitore BOF di ghisa ad alto tenore di silicio
MARINARI, ANDREA
2013/2014
Abstract
In the Basic Oxygen Steelmaking context, refining high-silicon hot metal is an awkward operation due to the significant tendency to slopping that it points out. At Steelworks n° 2 of ILVA steel plant situated in Taranto, this problem is solved by a double-slag operation. In the present work we have defined a new operating practice that, without the double-slag operation, achieves a reduction in the tap to tap time and a greater process gases recovery, without affecting the neither the slopping control nor the quality of steel obtained at the end of the blow. The feasibility of such a new practice was verified through a critical analysis of the results obtained from thirty experimental tests carried out at ILVA Steelworks n° 2 converters.File | Dimensione | Formato | |
---|---|---|---|
2014_07_Marinari.pdf
non accessibile
Descrizione: Testo della tesi
Dimensione
4.99 MB
Formato
Adobe PDF
|
4.99 MB | Adobe PDF | Visualizza/Apri |
I documenti in POLITesi sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.
https://hdl.handle.net/10589/93846