The scope of this experimental experience is to show the failure behaviour of composite slabs, formed by H60 profiled sheet, supplied by “O Feliz- Metalomecânica S.A” and lightweight concrete with LECA MD aggregates, supplied by Saint Gobain, Portugal. This study was led following the indications of UNI EN 1994-1-1:2005. The experimental program, conducted by tests at the “Laboratorio de Mecanica Estrutural” of the University of Coimbra, determined hypothetical m, k e τu,Rd values. The expression “hypothetical values” is used because the experimental campaign does not satisfy the minimum test number required by UNI EN 1994-1-1. Those empirical factors m, k e τu,Rd are mandatory to find the longitudinal shear resistance. The conduced tests show the common trend of the composite slabs to fail under longitudinal shear.

Lo scopo di questo lavoro sperimentale è presentare il comportamento a rottura di una piastra mista, costituita dalla lamiera grecata H60, fornita dall’impresa “O Feliz-Metalomecânica S.A.”, e da calcestruzzo alleggerito LECA MD, fornito da Saint Gobain, Portogallo. Lo studio è stato condotto utilizzando i requisiti presentati nel capitolo nove della UNI EN 1994-1-1:2005. Il programma sperimentale eseguito nel “Laboratorio de Mecanica Estrutural” dell’Università di Coimbra ha portato alla determinazione di ipotetici valori di m, k e τu,Rd tramite l’esecuzione di una serie di test. Si parla di “ipotetici” valori, in quanto la campagna sperimentale condotta non soddisfa il numero minimo di test richiesto dalla UNI EN 1994-1-1. Tali fattori empirici, m, k e τu,Rd, rientrano nella verifica di resistenza a taglio longitudinale. I test condotti rispecchiano la comune tendenza delle piastre miste a cedere per taglio longitudinale.

Composite slabs with lightweight concrete. Experimental evaluation of steel decking and lightweight concrete

PENZA, AURELIA
2009/2010

Abstract

The scope of this experimental experience is to show the failure behaviour of composite slabs, formed by H60 profiled sheet, supplied by “O Feliz- Metalomecânica S.A” and lightweight concrete with LECA MD aggregates, supplied by Saint Gobain, Portugal. This study was led following the indications of UNI EN 1994-1-1:2005. The experimental program, conducted by tests at the “Laboratorio de Mecanica Estrutural” of the University of Coimbra, determined hypothetical m, k e τu,Rd values. The expression “hypothetical values” is used because the experimental campaign does not satisfy the minimum test number required by UNI EN 1994-1-1. Those empirical factors m, k e τu,Rd are mandatory to find the longitudinal shear resistance. The conduced tests show the common trend of the composite slabs to fail under longitudinal shear.
ING VI - Facolta' di Ingegneria Edile-Architettura
21-lug-2010
2009/2010
Lo scopo di questo lavoro sperimentale è presentare il comportamento a rottura di una piastra mista, costituita dalla lamiera grecata H60, fornita dall’impresa “O Feliz-Metalomecânica S.A.”, e da calcestruzzo alleggerito LECA MD, fornito da Saint Gobain, Portogallo. Lo studio è stato condotto utilizzando i requisiti presentati nel capitolo nove della UNI EN 1994-1-1:2005. Il programma sperimentale eseguito nel “Laboratorio de Mecanica Estrutural” dell’Università di Coimbra ha portato alla determinazione di ipotetici valori di m, k e τu,Rd tramite l’esecuzione di una serie di test. Si parla di “ipotetici” valori, in quanto la campagna sperimentale condotta non soddisfa il numero minimo di test richiesto dalla UNI EN 1994-1-1. Tali fattori empirici, m, k e τu,Rd, rientrano nella verifica di resistenza a taglio longitudinale. I test condotti rispecchiano la comune tendenza delle piastre miste a cedere per taglio longitudinale.
Tesi di laurea Magistrale
File allegati
File Dimensione Formato  
2010_07_Penza.pdf

Open Access dal 28/06/2013

Descrizione: Testo della tesi
Dimensione 6.9 MB
Formato Adobe PDF
6.9 MB Adobe PDF Visualizza/Apri